Cut-edge corrosion

What is Cut-Edge corrosion?

Cut-edge corrosion is rust that begins at a cut in a coated steel sheet, where the steel is bare, and then creeps in under the coating.

In brief

A profiled metal roof sheet is steel with a protective coating. Wherever the sheet is cut, the coating stops and the steel shows at the edge. Moisture reaches that bare line, rust forms, and it spreads sideways under the paint. That is cut-edge corrosion. It shows at laps, sheet ends, rooflight openings and holes cut for pipes. Caught early it can be cleaned and treated, but once it has gone through the sheet, the sheet has to be replaced.

Why a cut leaves the steel exposed

A coated sheet is protected by a skin, not by the steel itself. The skin covers the faces of the sheet, and a clean factory edge or a site cut slices straight through it. At that thin line the steel is open to rain, to condensation and to whatever runs down the roof. Rust starts there because the barrier ends there.

Once rust takes hold it does not stay on the line. It undermines the coating from the side, lifts it in a blister and leaves the steel bare for a little further in, so the damage reaches beyond the mark you can see. A roofer reading the roof therefore looks past the orange line to the paint around it.

The worst edges are the ones cut on the roof itself, because a disc leaves swarf behind. Swarf is the fine metal dust and filings from the cut, and swarf left on the sheet rusts and stains the surface. A site cut that is brushed clean and sealed behaves better than one that is left as it fell. Our guide to cut-edge corrosion on metal sheets gives the longer version.

Where it shows on an industrial roof

A roof of profiled sheets always carries cut edges, and they gather in a handful of places. Each survey takes them in the same order, from the ground, from inside the unit and from a platform:

  • the lower ends of the sheets at the eaves, where they were trimmed to meet the gutter
  • the laps, where one sheet edge lies against the next
  • the openings cut for rooflights, fans, flues and pipes
  • the ends against the ridge, the verge and the end walls
  • sheets shortened on site because a stock length did not fit

Signs from the ground are an orange line along a lap, flaking or blistered paint at an end, and rust streaks running down from a rooflight opening. Inside the building, brown stains on the lining, dark patches on insulation and pin points of daylight tell you the rust has already gone through. Daylight is the plainest warning, because it means the steel has been lost, not merely stained.

None of this needs a climb to spot, and binoculars and a torch inside the unit do most of the first look.

Rusty edge or rusty fixing: telling them apart

Several faults leave an orange stain on a steel roof, and treating the wrong one achieves nothing. Before anything is named cut-edge corrosion, the others are ruled out:

  • a rusting screw head or washer on a sheet that is otherwise sound, which our answer on rusting roof sheet fixings covers
  • condensation dripping from the cold underside of the sheet, covered in the answer on why a metal roof drips inside
  • an overflowing gutter that keeps the lowest edge of the sheet wet
  • moss and debris sitting in a lap and holding moisture against the paint
  • scratches from ladders, tools and earlier trades, which behave like small cuts

The point is where the rust begins. If it starts at a sheared edge and works inwards, it is cut-edge corrosion. If it starts at a screw and spreads outwards, it is a fixing problem, and if the underside is wet while the top is dry, look to condensation. A single roof can have all three, and the survey records each one separately with its own photographs.

Treating it, and the rules either side of the border

The choice depends on how far the rust has travelled. Light rust at a lap can be cleaned back and coated. Sheets that have lost metal are replaced. A roof that is failing everywhere may be better re-covered, which means a new sheet fixed over or instead of the old. A coat of paint on rust that has spread beneath the old coating only postpones the failure.

A job that grows into re-covering meets the Building Regulations, and the two sides differ:

  • In England, the Planning Portal, writing for houses, states that an application is not normally needed where "Less than 25 per cent of the total 'building envelope'" and "Less than 50 per cent of the roof" is affected.
  • In Wales, the Welsh Government says of re-roofing: "In most situations, this work will need Building Regulations approval."

For a unit, building control says which test applies. If any sheet in the roof is asbestos cement, HSE says "AC roofs are always fragile", so access is planned first. Our commercial roofing page explains how a survey becomes one written total price, scaffold included.

Related questions

Can I paint over cut-edge rust myself?

Painting hides the problem without stopping it if rust has already moved under the coating. The edge needs cleaning back to sound metal first, and the sheets are not safe to walk. A damp steel sheet is slick underfoot and may be thin where rust has gone through, so the work is done from a platform or behind edge protection.

Does rust at a rooflight opening mean the whole roof is failing?

Not by itself. An opening has a long cut edge, so rust can show there. The survey looks at the other laps and sheet ends before saying whether this is a local repair or a wider fault. You see the photographs of each edge on your own roof, and the written quote follows.

Get your free roof quote

Tell us about the roof and we will arrange a survey.

10-year workmanship guarantee, in writing