01432 610152 Get a quote Call 01432 610152

GRP cracks

Why does a GRP roof crack?

A GRP roof is a rigid shell over a timber deck, and it cracks where the deck moves more than the shell can bear, or where something strikes it.

Short answer

GRP sets hard, so it cannot stretch. A crack can mark a place where something underneath has moved: a board joint, an edge, or a deck that flexes underfoot. Other cracks come from a knock, from a topcoat that has aged, or from a layer of fibreglass laid too thin. Where the crack sits and which way it runs tells us which cause we are dealing with.

Reading a crack by its shape and position

Cracks in a fibreglass roof are not all the same, and their shape is the best clue we have. This table sets out what each pattern can point to. It lists possibilities, so each one is checked against the rest of the roof before we name a cause, and a single crack may not tell the whole story on its own.

What different cracks on a GRP roof can mean
PatternWhat it looks likeWhat it can point to
Straight lineFollows the joint between two boardsMovement in the deck
Fine networkCrazing across the topcoatA topcoat that has aged or is thin
Star or crescentRadiates from one pointAn impact, such as a dropped tool or a foot
Line along an edgeRuns beside a trim or wallMovement where the roof meets a rigid detail

A crack that is only in the topcoat is a surface matter. A crack that goes through to the glass fibres lets water reach the deck, which makes it a leak waiting to show.

Why the deck decides what the shell does

Timber is not still. A board takes up moisture and swells, then dries and shrinks, and a deck made of several boards or sheets moves along its joints as it does. Rigid GRP laid over that movement has nowhere to go, so it splits along its weakest line, and a board joint is a natural one.

Flexing is the other cause. A deck that is too thin, or spans too far between joists, bounces a little when someone walks on it. GRP does not mind the weight, but it minds the bounce. Over time a hairline opens where the flex is greatest.

Deck movement is one reason a GRP roof may fall short of a quoted range, and our page on how long GRP lasts sets HomeBuilding's 25-30 years beside Less's 25 to 40. The detail of how a new GRP roof is built to avoid these problems, from the boards upward, is on GRP fibreglass flat roofs.

When we find a crack along a board joint, we press the boards either side to feel for movement, then photograph the crack with a ruler laid beside it for scale.

Other causes: thin laminate, topcoat wear and knocks

Not every crack starts underneath. Three other causes come up on a survey.

  • A laminate laid too thin. The layers of resin and glass matting give the shell its strength, and where they are thin, the shell can crack under ordinary use.
  • A topcoat worn by sun and weather. As it thins, crazing appears on the surface and the resin beneath begins to chalk.
  • Impact. A dropped tool, a ladder foot or a branch can crack the shell at a single point.

Sometimes the cause cannot be read from the surface alone, and in that case we say plainly that it is uncertain and set out what we would check next, such as lifting a small test area.

The fix follows the cause. A local crack in a sound deck can be cut out and laminated again. Widespread crazing may call for a fresh topcoat. On cost, Checkatrade's repair rates (June 2026) for GRP fibreglass are £130 to £180 per m², ex VAT, applied to patches no larger than 3 m². Where cracks run across the whole roof, our guide to patching or replacing helps you weigh a re-lay.

When a cracked GRP roof needs more than a repair

A re-lay becomes the honest answer when the deck is the problem. If the boards are soft, stained or sagging, new resin on top fixes nothing, because the movement that cracked the old shell will crack the new one. The deck is repaired or replaced first, and the shell goes on after.

A full re-lay is also renovation of the roof, so the rules come in. In England, the Planning Portal sets its test at less than 25 per cent of the building envelope and less than 50 per cent of the roof, and Table 4.3 of Approved Document L (2021 edition) gives 0.35 and 0.16. In Wales, the Welsh Government's guidance begins from approval being needed for re-roofing in most situations, and Table 11.1 of the Welsh Approved Document L asks for 0.16, with 0.35 as the worst acceptable figure.

We ask the council's building control service, or a registered building control approver, which of these governs your address, and then give you one written total price. The flat roofing hub links to the rest of the flat roof guides.

Related questions

Is a hairline crack in GRP always a leak?

No. A crack confined to the topcoat is a surface line, and the glass layer below can still be sealed. One that runs through to the fibres can let water in. We look at it up close, check how it behaves when the surface is damp, and photograph what we see before saying which kind it is.

Can new resin be brushed over cracks to stop them?

For a surface line in a sound deck, a repair can work. If the crack comes from deck movement, it tends to reopen because the cause is still there. We look for the movement first, and show you the boards and the joint so you can see why a surface fix would or would not last.

Get your free roof quote

Tell us about the roof and we will arrange a survey.

10-year workmanship guarantee, in writing